Inclusion (encapsulated ) Cadmium Orange MY9001 MY9002 |
»óÇ°ºÐ·ù: |
¿°·á°ú ¾È·á
|
µî·ÏºÐ·ù: |
Offer to Sell |
³»¿ë: |
Additional_detail: MY9001 MY9002 MY9003
Inclusion (encapsulated )Orange
component: Se-Cd-Zr-Si
firing stability:up to 1300'c
(2372'F)
Application hints :
1 .better results with high
refractive index ftitted glaze.
2.best results with no Zinc
Oxide,not suitable for Zirconium
opacified glaze.
3. Glazes systems containing
Alkali metals (<5% weight)
improve the color development of
pigment inclusion.
4.Component of SiO2 in glazes
should below 50% (weight).
5. An appropriate amount of PbO
added in the glaze can increase
the brightness and lightness of
color.
6.To avoid mechanical destruction
of inclusion pigment during glaze
preparation, we recommend adding
the pigment when only 5% of the
total milling time remains.
|
¿¬¶ôó |
´ã
´ç ÀÚ: |
Jackie Liu |
ȸ»çÁÖ¼Ò: |
Room No 306,10th Building, 5th Liuyuan Street, Shiwan Town |
ÀüȹøÈ£: |
86-757-82712858 |
Æѽº¹øÈ£:
|
86-757-82709177 |
E - mail: |
jackieliu0909@hotmail.com |
|